A professional-grade mortar mix enhanced with acrylic polymers for improved flexibility and adhesion. Ideal for fast-track construction projects and repairs, this formulation is suitable for both wet and dry environments, ensuring durability and performance.
Technical Specifications
pH Level: 12-13
Shelf Life: 12 months in a sealed container
Batch Size: 1000 kg batch
Processing Time: 45-60 minutes
Temperature: 15-25°C
Storage: Store in a cool, dry place away from direct sunlight and moisture.
Viscosity: Medium to high viscosity suitable for trowel applications
Certification: ISO 9001:2015, ASTM C270
Ingredients
Ingredient
Percentage
Function
Portland Cement
50.0%
Primary binding agent
Silica Sand
30.0%
Provides structural integrity and texture
Acrylic Polymer
10.0%
Enhances adhesion and elasticity
Calcium Aluminate
5.0%
Accelerates setting time
Hydrated Lime
3.0%
Improves workability and water retention
Water Reducing Agent
1.5%
Reduces water demand and improves flow
Defoamers
0.5%
Minimizes air entrainment for smoother application
Manufacturing Process
Dry Blend Phase
Mix Portland Cement and Silica Sand thoroughly in a large mixer.
Add Calcium Aluminate and Hydrated Lime to the mixture.
Ensure even distribution of dry ingredients through consistent mixing.
Wet Blend Phase
In a separate container, mix Acrylic Polymer with the Water Reducing Agent.
Add the wet mixture to the dry blend slowly, while continuously mixing.
Introduce Defoamers into the mixture, ensuring no air bubbles form.
Usage Instructions
Mix the formulated mortar with clean water at a ratio of 4:1 (mortar to water) before application. Apply to the desired surface within 20 minutes of mixing to ensure optimal performance.